Artigos de Revista
Info
A novel technique for the interface characterisation of glass fibre-polypropylene systems
In the present work, a new technique was developed to determine the interfacial properties of two opaque glass fibre/polypropylene (GF/PP) systems via fragmentation tests on single filament model composites. Fragmentation tests usually require the fibre inside the composites to be completely aligned in the loading direction. Since PP matrices are non-transparent, it is not possible to guarantee a priori this condition. Hence, a novel technique was developed to determine the inclination of the filaments embedded in the composites. The fibrepolymer systems were also evaluated by comparing their interfacial properties with the overall mechanical properties determined on pultruded GF/PP composites. The present work shows that the knowledge of the interfacial properties is important, not only to compare alternative fibre/matrix systems, but also to assess whether the level of adhesion in these systems is adequate to fabricate composites with good mechanical properties.
Ano: 2003
Número Páginas:
907-913pp.
Autor(es): Cabral-Fonseca, S.; M.C. Paiva; Nunes, J. P.; C.A. Bernardo
Revista: Polymer Testing
Editor: Elsevier
Volume:
22.
Keywords: Composites; Mechanical properties; Fragmentation; Adhesion; Interfacila properties
Info
Artificial Simulated and Natural Weathering of Poly(vinyl Chloride) for outdoor applications: the evolution of the mechanical and molecular properties
The low cost and the good performance of poly(vinyl chloride) products make this polymer very suitable for applications in buildings, mainly in exterior applications, like window profiles, cladding structures and siding. However, the ultimate user acceptance of PVC products for outdoor building applications will depend on their ability to resist the deterioration of their mechanical and aesthetic properties over long periods of exposure. In order to assure the weatherability of these materials, the PVC resin needs to be compounded and processed properly, using suitable additives, leading to a complex material, whose behaviour and properties are quite different from the PVC resin by itself. The outdoor degradation of such products is complex and not completely understood for most of the technical formulations, so the study of the photodegradation of such products still remains a matter of interest. In the present work, we have used various analytical techniques to evaluate the variations of the physical,chemical and mechanical properties of extruded PVC samples, resulting from the degradation by light.
Ano: 2003
Número Páginas:
235-243pp.
Autor(es): Real, L. P.; Rocha, A.; Gardette, Jean-Luc
Editor: ELSEVIER
Volume:
82.
Keywords: Mechanical properties; Colorimetry; Infrared microscopy; Weathering; Poly(vinyl chloride)
Info
Production of powder-coated tpwpregs and composites
Na eficiente and cost-effective dry coating process was developed to deposit polymer powders on continuous fibers and produce thermoplastic matrix towpregs to be processed into composites. The technological solutions used in the coating line construction and the influence of the precessing parameters on manufactured glass fibre reinforced polypropylene (GF/PP) towpregs are detailed in this paper.Composites were produced from characterized GF/PP towpregs using hot plate compression moulding. The mechanical properties determined on the composites are compared with theoretical values predicted by the Classical Laminate Theory using the experimentally determined raw material contentes and tensile properties.
Ano: 2003
Número Páginas:
231-248pp.
Autor(es): Nunes, J. P.; J. F. Silva; A.T. Marques; N. Crainic; Cabral-Fonseca, S.
Revista: Journal of Thermoplastc Composite Materials
Editor: Sage Publications
Keywords: Mechanical properties; Compression moulding; Polypropylene; Glass fiber; Long fiber composites; Reinforced thermoplastics; Towpregs; Powder-coating process
Info
Ageing and Characterisation of PVC based compounds utilised for Exterior Applications in the Building Construction Field. Part 2: Artificial accelerated ageing with xenon light
This set of articles describes the behaviour of formulated polyvinylchorides in various conditions of photoageing, including exposition in artificial and in natural conditions. In this article, the modification of the infrared and UVvisible spectra of PVC films irradiated with a xenon light are reported
Ano: 2001
Número Páginas:
789-794pp.
Autor(es): Real, L. P.; Gardette, Jean-Luc
Editor: ELSEVIER
Volume:
20.
Info
Ageing and Characterisation of PVC-based compounds utilised for Exterior Applications in the Building Construction Field. Part 1: Thermal ageing
One major problem encountered with polymeric materials is their sensitivity to outdoors weathering. Exposure to outdoors conditions leads to a degradation of the use properties of the material. This set of articles describes a comparison of the behavior of several stabilised polyvinylchlorides exposed to various conditions of ageing including light and temperature. The first article focusses on the effect of thermal ageing on the infrared and UV-visible characteristics of the selected samples.
Ano: 2001
Número Páginas:
779-787pp.
Autor(es): Real, L. P.; Gardette, Jean-Luc
Editor: ELSEVIER
Volume:
20.
Keywords: Uv-visible spectroscopy; Infrared spectroscopy; Thermal ageing; Pvc
|
Comunicações
Info
Environmental degradation of gfrp pultruded profiles made of polyester and vinylester resins
This communication presents preliminary results of a research project on the effects of different environmental agents on the physical, chemical, aesthetical and mechanical properties of glass fibre reinforced polymer pultruded (GFRP) profiles made of either polyester or vinylester resin. In order to study the potential degradation of the two types of profiles in typical environments of civil engineering applications, test specimens are being subjected to the following exposure conditions: (i) immersion in demineralised water, at 23 ºC, 40 ºC and 60 ºC; (ii) immersion in salt-water, at the same temperatures; (iii) continuous condensation at 40 ºC; (iv) salt fog chamber; (v) thermal cycles, from -5ºC to 40ºC; (vi) accelerated weathering fluorescent ultraviolet light apparatus. Additionally, test specimens were placed in the roof of LNEC thereby being subjected to a natural degradation in a controlled environment. At predefined time intervals, batches of test specimens placed in the above mentioned exposure environments are being removed for physic-chemical and mechanical characterization, in order to assess their behaviour. / Nesta comunicação são apresentados os resultados preliminares de um projecto de investigação em que estão a ser avaliados os efeitos da degradação ambiental nas características físico-químicas de perfis pultrudidos de plástico reforçado com fibra de vidro com dois tipos de matriz uma de poliéster e outra de viniléster. Com o objectivo de estudar os eventuais efeitos de degradação nos dois tipos de perfis, quando expostos a condições típicas das aplicações em engenharia civil, foram efectuadas as seguintes exposições em provetes retirados dos perfis: (i) imersão em água desmineralizada, a 23 ºC, 40 ºC e 60 ºC; (ii) imersão numa solução salina, às mesmas temperaturas; (iii) condensação em contínuo a 40 ºC; (iv) câmara de nevoeiro salino; (v) ciclos térmicos, entre -5 ºC e 40 ºC; (vi) envelhecimento artificial acelerado com lâmpadas fluorescentes de radiação ultravioleta. Para além disso, foram expostos provetes no telhado do edifício principal do LNEC, onde ficaram sujeitos a envelhecimento natural. Em intervalos predefinidos, foram efectuados ensaios de caracterização físico-química e mecânica dos materiais, para monitorizar o seu desempenho ao longo do tempo.
Ano: 2009
Número Páginas:
22pp.
Autor(es): Cabral-Fonseca, S.; Correia, J.; Costa, R.; Carreiro, A.; Rodrigues, M. P.; Eusébio, M. I.; Branco, F.
Editor: LNEC
Keywords: Atmospheric corrosion; Thermal degradation; Construction materials degradation; Polyester resin; Reinforced plastic; Glass fibre; Construction profile
Info
Jornadas da APAL 2009 Qualisteelcoat
N/A
Ano: 2009
Número Páginas:
4p.
Autor(es): Eusébio, M. I.
Info
Study of the influence of the ageing conditions in the durability of PVC formulations used in outdoor applications
The main purpose of this paper is to present the results of a study intended to assess the durability of stabilized PVC-U for outdoor applications, in form of calendered films and extruded plates. The samples were subject to different ageing conditions and their degradation state were evaluated, using techniques of molecular analysis, namely Fourier transformed infrared spectroscopy (FTIR), as well techniques for evaluation of macroscopic properties, as colorimetry and tensiles tests. The development of formulations, the ageing and the subsequent characterisation were done in LNEC. Therefore, after a brief introduction, this paper presents the experimental part of the study, as regards the composition of samples and the experimental methods of deterioration and characterisation. Subsequently, the results of the study, their interpretation and the final conclusions are also presented.
Ano: 2008
Número Páginas:
35.
Autor(es): Real, L. P.
Editor: LNEC
Keywords: Experimental test; Degradation of construction materials; Ageing of construction materials; Durability of construction materials; Pvc
Info
Study of the influence of the ageing conditions in the durability of PVC formulations used in outdoor applications
The main purpose of this paper is to present the results of a study intended to assess the durability of stabilized PVC-U for outdoor applications, in form of calendered films and extruded plates. The samples were subject to different ageing conditions and their degradation state were evaluated, using techniques of molecular analysis, namely Fourier transformed infrared spectroscopy (FTIR), as well techniques for evaluation of macroscopic properties, as colorimetry and tensiles tests. The development of formulations, the ageing and the subsequent characterisation were done in LNEC. Therefore, after a brief introduction, this paper presents the experimental part of the study, as regards the composition of samples and the experimental methods of deterioration and characterisation. Subsequently, the results of the study, their interpretation and the final conclusions are also presented.
Ano: 2008
Número Páginas:
44pp.
Autor(es): Real, L. P.
Editor: LNEC
Keywords: Ageing of construction materials; Pvc; Durability of construction materials; Degradation of construction materials
Info
Degradation studies of PVC films
The outdoor degradation of poly(vinyl chloride) (PVC) products is complex and not completely understood for most of the technical formulations. Furthermore, it is known that the behaviour of such materials is dependent of the photo-oxidation conditions, namely source of radiation, temperature, presence of water and humidity. In the present work, we have used X-ray photoelectron spectroscopy (XPS) to evaluate the influence of different photo-oxidation conditions on the surface degradation of stabilized PVC, low thickness calendered samples (~ 150 ?m). The main objective is the study of the influence of the weathering conditions on the degradation level of stabilized PVC products for outdoor applications trying to go deeper in the understanding of the mechanism of both the degradation and the stabilization of the surface under different environmental conditions, different polymer formulations and different processing methods (extrusion or calendering). Comparisons are made with previous results obtained using colourimetry and infrared spectroscopy. The role of PVC formulation and of radiation source and water were studied using artificial weathering. Results were compared with degradation induced by natural weathering in Lisbon.
Ano: 2007
Número Páginas:
1.
Autor(es): Rego, A. M. B.; A.M. Ferraria; Real, L. P.
Info
Artificial accelerated weathering of PVC for outdoor applications: The evolution of physical and mechanical properties
The main purpose of this paper is to present the results obtained, during the years 2001 and 2002, from a study developed in LNEC. The object of this study was to assess the synergetic effect of three of the most significant deteriorating climatic agents (radiation, temperature and water) on the evolution of the properties of hard PVC stabilised with titanium dioxide, for outdoor applications. For the purpose, several samples were subject to natural and artificial weathering. Moreover, their physical and mechanical properties were characterised by techniques of analysis and assessment of the surface aspect (colour and brightness), of assessment of the molecular properties by infrared microscopy (MICROFTIR), as well as of determination of the tensile mechanical properties and assessment of the Charpy impact resistance. The paper was both orally presented and by poster at the panel meeting Ageing, Irradiation, Stabilisation of the Congress MoDeSt 2002. Therefore, this publication includes the text of the paper, the poster, as well as the slides from the oral communication. The development of the formulations, the ageing and the subsequent characterisation by colorimetry, brightness, Charpy impact and tension, were done in LNEC. The characterisation by infrared microscopy was performed in the Laboratoire de Photochimie Moleculaire et Macromoleculaire of the University Blaise-Pascal, Clermont-Ferrand, France.
Ano: 2006
Número Páginas:
37 pp.
Autor(es): Real, L. P.; Rocha, A.; Gardette, Jean-Luc
Editor: LNEC
Keywords: Colorimetry; Infrared microscopy; Natural weathering; Mechanical characterization; Physical characterization; Accelerated weathering; Pvc
Info
Artificial simulated and natural weathering of PVC for outdoor applications: The influence of radiation and water in the evolution of PVC properties
The main purpose of this paper is to present the results obtained, during the year 2003, from a study developed in LNEC. The object of this study was to assess the synergetic effect of two deteriorating climatic agents (radiation and water) on the evolution of the properties of extruded plates made of hard PVC stabilised with titanium dioxide, for outdoor applications. For the purpose, several samples were subject to natural and artificial weathering, their deterioration condition having been characterised by means of techniques of analysis of colorimetry and infrared spectroscopy (FTIR). Initially, only the presentation of a poster titled Artificial and Natural Weathering of Polyvinyl chloride for Outdoor Applications: the Influence of the Radiation and Water on the Evolution of the PVC Properties was scheduled. Nevertheless, upon request from the secretariat of the Congress, the author also presented an oral paper on the same subject, but including experimental results obtained during the year 2004, which were not mentioned in the poster. Similarly, these results, which were obtained by means of surface analysis techniques by Scanning Electron Microscopy (SEM) and by X photoelectron spectroscopy (XPS), were not included in the paper submitted to the Congress. Therefore, this publication includes the text of the paper referring to the poster, which was initially predicted, as well as the slides of the oral communication presented. It also contains a few results obtained in 2004. The development of the formulations, as well as the ageing and the subsequent characterisation by colorimetry, by infrared spectroscopy and by scanning electron microscopy were performed in LNEC. The characterisation by X photoelectron spectroscopy was conducted at the Molecular Chemistry-Physics Centre of the Instituto Superior Técnico (Higher Technical Institute).
Ano: 2006
Número Páginas:
23 pp.
Autor(es): Real, L. P.; Rocha, A.; Gardette, Jean-Luc; Rego, A. M. B.
Editor: LNEC
Keywords: Electronic spectroscopy; Colorimetry; Infrared microscopy; Scanning electron microscopy; Accelerated weathering; Natural weathering; Pvc
Info
The Influence of Weathering Conditions in the Evolution of Molecular Properties of Poly(Vinyl Chloride) for Outdoor Applications. An Analytical Study Using Techniques of Surface Analysis (SEM and XPS)
The main purpose of this paper is to present the results of a study intended to assess the deterioration condition of extruded hard PVC plates, for outdoor applications. The plates were subject to different ageing conditions, using techniques of surface analysis, namely scanning electron microscopy (SEM) and X-ray photoelectron spectroscopy (XPS). The development of formulations, the ageing and the subsequent characterisation by scanning electron microscopy were done in LNEC. The characterisation by X-ray photoelectron spectroscopy was done at the Centre for Molecular Chemistry-Physics of Instituto Superior Técnico (Higher Technical Institute of Lisbon). Therefore, after a brief introduction, this paper presents the experimental part of the study, as regards the composition of samples and the experimental methods of deterioration and characterisation. Subsequently, the results of the study, their interpretation and the final conclusions are also presented.
Ano: 2006
Número Páginas:
28.
Autor(es): Real, L. P.; Rego, A. M. B.
Editor: LNEC
Keywords: Spectroscopy of photoelectron x; Surface analysis; Electronic spectroscopy; Scanning electron microscopy; Weathering of construction materials; Degradation of construction materials; Pvc
Info
Validação de programa informático para calibração de um calorímetro diferencial de varrimento e incerteza associada à determinação da entalpia de fusão
Procurou-se com a presente comunicação, apresentar uma metodologia de validação de um programa informático, desenvolvido no NMPC do LNEC especificamente para a calibração de um calorimetro diferencial de varrimento (DSC) e para calcular a incerteza associada à determinação da entalpia de fusão. Assim, após uma breve introdução, a presente comunicação expõe a formulação essencial que serviu de suporte ao desenvolvimento do programa informático referido, descreve os elementos que constituem o procedimento de validação do mesmo, apresenta o processo de estimativa da incerteza de medição e os resultados da análise efectuada.
Ano: 2006
Número Páginas:
21.
Autor(es): Real, L. P.; Ribeiro, A.
Editor: LNEC
Keywords: Fusão; Entalpia; Calorimetria diferencial de varrimento; Incerteza de medição; Software; Calibração; Calorímetro
|
|
Capítulos de Livros
Renovação da Marca de Qualidade Qualicoat, 2011. Inspecção de 14-07-2011 à empresa J. Silva & Cª. - Licença P-822
|
|
|
Relatórios
Info
Regras para a concessão de documentos de aplicação a revestimentos por pintura elastoméricos para rebocos de cimento e para betão em superfícies exteriores de edifícios
No presente relatório descrevem-se os procedimentos adotados pelo LNEC, no âmbito do estudo a efetuar para a concessão de um Documento de Aplicação (DA), relativo a revestimentos por pintura elastoméricos para rebocos de cimento e para betão aplicados em paredes exteriores de edifícios. Consideram-se as condições de exposição atmosférica no exterior sem a influência de ações químicas severas. Indicam-se, também, as ações a desenvolver periodicamente para comprovar que continuam reunidas as condições que terão permitido a concessão do DA.
Ano: 2021
Autor(es): Silva, H. M.; Cabral-Fonseca, S.; Rodrigues, M. P.
Keywords: Rebocos de cimento e betão; Superfícies exteriores; Revestimentos por pintura elastoméricos; Documento de aplicação
Info
Regras para a concessão de Documentos de Aplicação a revestimentos por pintura de base aquosa para superfícies interiores de habitações paredes e tetos
No presente relatório descrevem-se os procedimentos adotados pelo LNEC para a concessão de um Documento de Aplicação (DA) relativo a revestimentos por pintura de base aquosa para aplicação em paredes e tetos de interiores de habitações, sobre superfícies de estuque de gesso, de gesso cartonado, de reboco de cimento ou de betão. Indicam-se, também, as ações a desenvolver periodicamente para comprovar que continuam reunidas as condições que permitiram a concessão do DA.
Ano: 2018
Autor(es): Cabral-Fonseca, S.; Rodrigues, M. P.
Keywords: Paredes e tetos; Superfícies interiores; Revestimentos por pintura; Documento de aplicação
Info
Estação Meterológica do LNEC Compilação de dados Ano 2016 - Edifício Principal Terraço da Ala Nascente
No presente relatório apresentam-se os dados meteorológicos do ano de 2016 recolhidos na estação meteorológica existente no Núcleo de Materiais Orgânicos do Departamento de Materiais do LNEC, em Lisboa
Ano: 2017
Autor(es): Cabral-Fonseca, S.
Keywords: Ano 2016; Dados meteorológicos; LNEC
Info
Regras para a concessão de documentos de aplicação a revestimentos por pintura para rebocos de cimento e para betão em superfícies exteriores
No presente relatório descrevem-se os procedimentos adotados pelo LNEC no âmbito do estudo a efetuar para a concessão de um Documento de Aplicação (DA) relativo a revestimentos por pintura para rebocos de cimento e de betão aplicados em superfícies exteriores (tintas não elastoméricas). Consideram-se as condições de exposição atmosférica no exterior, sem influência de ações químicas severas. Indicam-se, também, as ações a desenvolver periodicamente para comprovar que continuam reunidas as condições que terão permitido a concessão do DA. Este relatório constitui uma revisão do relatório do LNEC nº 252/2013-DM/NMO.
Ano: 2017
Autor(es): Cabral-Fonseca, S.; Rodrigues, M. P.
Keywords: Rebocos de cimento e betão; Superfícies exteriores; Revestimentos por pintura; Documento de aplicação
Info
Estação meteorológica do LNEC - Compilação de dados Ano de 2014 Edifício Principal Terraço da Ala Nascente
No presente relatório apresentam-se os dados meteorológicos do ano de 2014 recolhidos na estação meteorológica existente no Núcleo de Materiais Orgânicos dom Departamento de Materiais do LNEC, em Lisboa
Ano: 2015
Autor(es): Cabral-Fonseca, S.
Keywords: Ano 2014; LNEC; Dados meteorológicos
Info
Estação meteorológica do LNEC - Compilação de dados ano 2013 Edifício Principal Terraço da ala Nascente
No presente relatório apresentam-se os dados meteorológicos do ano de 2013, recolhidos na estação meteorológica existente no Núcleo de Materiais Orgânicos do Departamento de Materiais do LNEC, em Lisboa.
Ano: 2014
Autor(es): Cabral-Fonseca, S.
Keywords: Ano 2013; LNEC; Dados meteorológicos
Info
Regras para concessão de documentos de aplicação a produtos de revestimentos de superfícies de madeira em condições de exposição no exterior
No presente relatório descrevem-se os procedimentos adoptados pelo LNEC no âmbito dos estudos para concessão de um Documento de Aplicação (DA) a produtos de pintura para proteção de superfícies madeira, em condições de exposição atmosférica no exterior. Indicam-se também as ações a desenvolver periodicamente para comprovar que continuam reunidas as condições para a concessão do DA.
Ano: 2013
Número Páginas:
26pp.
Autor(es): Rodrigues, M. P.
Editor: LNEC
Info
Sistemas de tubagem de poli(cloreto de vinilo) não plastificado (PVC-U) destinados à extração de água em profundidade - Critério para avaliação da aptidão ao uso, com vista à concessão de homologação
Nesta publicação apresenta-se o critério presentemente seguido pelo LNEC para concessão de homologação com certificação, bem como posterior controlo periódico da qualidade a sistemas de tubagem de poli(cloreto de vinilo) não plastificado (PVC-U) destinados à extração de água em profundidade. Após uma breve introdução e a definição do objetivo, indicam-se: - Os requisitos para o sistema da qualidade seguido pelo fabricante; - as caraterísticas e as especificações para a matéria-prima constituinte dos tubos e acessórios; - as caraterísticas e as especificações para os produtos finais, designadamente os tubos e as suas uniões; - a classificação das condições de serviço; - as recomendações para a utilização dos produtos, relativamente ao seu transporte e manuseamento, armazenagem e instalação; - os requisitos do LNEC para o autocontrolo do fabricante; - os requisitos de amostragem do LNEC durante as auditorias técnicas ou campanhas de recolha realizadas ao fabricante pelos técnicos do LNEC, no âmbito da concessão e manutenção da homologação.
Ano: 2013
Número Páginas:
27pp.
Autor(es): Real, L. P.
Editor: LNEC
Info
Avaliação da qualidade de tubagem de polietileno de alta densidade incorporando material reciclado - Avaliação de propriedades de híbridos do polietileno reciclado de alta densidade com nanoargilas
O presente relatório (relatório 2) contém os resultados de um estudo desenvolvido no Núcleo de Materiais Orgânicos (NMO) inserido num projeto de Pós-Doutoramento com a duração de três anos e teve como objetivo a avaliação do melhoramento das propriedades fisicas e mecânicas de amostras de polietileno reciclado em misturas binárias com nanoargilas ligantes (nanoclays), para aplicação em tubagem na construção civil. Assim, após uma caracterização preliminar de reciclados de polietileno (relatório 1) e antes da análise do desempenho de tubagem incorporando material reciclado (relatório 3), realizou-se um estudo de otimização de formulações introduzindo materiais cerâmicos constituídos por silicatos e aluminatos (nanoargilas) com o objetivo de melhorar algumas propriedades térmicas e mecânicas da matéria-prima. Com diversas técnicas de análise, estando entre elas a calorimetria diferencial de varrimento, a análise mecânica-dinâmica e a termogravimetria, obtiveram-se resultados experimentais que foram analisados a nível estrutural.
Ano: 2012
Número Páginas:
101pp.
Autor(es): Sampaio, M. O.
Editor: LNEC
Info
Avaliação da qualidade de tubagem de polietileno de alta densidade incorporando material reciclado - Avaliação do desempenho e da degradação do polietileno reciclado em tubagem de plástico
O presente relatório, que é o último de uma série de 3, contém resultados de um estudo desenvolvido no Núcleo de Materiais Orgânicos (NMO) da instituição de acolhimento LNEC, inserido num projeto de Pós-Doutoramento, subsidiado pela FCT. O objetivo foi o de avaliar o desempenho e a degradação de tubos incorporando polietileno reciclado, proveniente da indústria portuguesa. Recorrendo à calorimetria diferencial de varrimento foram medidos o tempo e a temperatura de indução à oxidação de compostos granulados usados para o fabrico de tubos, bem como de amostras extraídas de tubos. Através de ensaios de resistência à pressão interior foram caracterizados tubos extrudidos laboratorialmente, utilizando amostras de PEADRepsol PE T1OONN e amostras recicladas, tal como suas misturas percentuais com masterbatch contendo nano argila e antioxidante.
Ano: 2012
Número Páginas:
86pp.
Autor(es): Sampaio, M. O.
Editor: LNEC
|
Informações Científicas e Técnicas
Info
Estatística de ensaios interlaboratoriais - Tratamento e avaliação de resultados experimentais
Os resultados experimentais, obtidos através da medição de propriedades dos materiais e produtos, requerem tratamento específico e adequado, de forma a garantir a sua qualidade. É por isso muitas vezes necessário recorrer a métodos estatísticos para fazer a análise do tipo de distribuição dos resultados, proceder à deteção de valores suspeitos num conjunto de observações e à eventual rejeição de resultados anómalos. Este tipo de tratamento estatístico é principalmente adequado a ensaios de intercomparação, quer do foro metrológico (comparação de valores de padrões ou materiais de referência, mediante medição efetuada por operadores de diferentes laboratórios metrológicos, com incerteza variável), quer do âmbito dos laboratórios de ensaio. Os ensaios de Comparação Interlaboratorial realizados por laboratórios de ensaio, constituem uma ferramenta de garantia da Qualidade e são utilizados para a validação de métodos de ensaio (incerteza e robustez) e como um meio para a determinação das características de desempenho dos laboratórios, nomeadamente da reprodutibilidade e da repetibilidade. Nesta publicação faz-se uma descrição dos vários parâmetros que devem ser determinados em ensaios interlaboratoriais do tipo Intercomparações com valor de consenso e respetivos métodos de cálculo. A estatística aqui apresentada pode, numa boa parte dos casos, ser também aplicada à análise de resultados de medições experimentais correntes.
Ano: 2015
Autor(es): Real, L. P.
Keywords: Garantia de qualidade; Método estatístico; Ensaio interlaboratorial
Info
Weathering and polymer degradation - Review article
The main purpose of this Paper is to present a state of the art about weathering and polymer degradation. This review was presented during a training course promoted by the 5th European Weathering Symposium EWS (XXVIIth Colloquium of Danubian Countries on Natural and Artificial Ageing of Polymers), which was held in Lisbon on September 21 - 23, 2011, organised on behalf of CEEES (Confederation of European Environmental Engineering Societies) by the German Management Society for Environmental Engineering GUS (Gesellschaft für Umweltsimulation e.V.) and supported by SOPSAR (Sociedade Portuguesa de Simulação Ambiental e de Avaliação de Riscos), APIP (Associação Portuguesa da Indústria de Plásticos) and LNEC (Laboratório Nacional de Engenharia Civil). The main topics of this review are the weathering of polymers and composites, the determination, simulation and effects of relevant climatic quantities, innovative polymer additives, new test procedures and devices, instrumental methods of analysis to evaluate polymer degradation, recent developments in polymeric materials and composites designed for outdoor applications and methods for service-life prediction.
Ano: 2012
Número Páginas:
135pp.
Autor(es): Real, L. P.
Editor: LNEC
Keywords: Durability of construction materials; Construction materials degradation; Materials construction weathering; Composite materials; Polymer
|
|
Outros
Info
MILACRIL BRILHANTE (cor branca) e PRIMÁRIO TT - Revestimento por pintura para azulejos em paredes e tetos interiores de habitações
N/A
Ano: 2022
Autor(es): entidade LNEC
Keywords: Documento de aplicação; Revestimento de paredes; Revestimento por pintura; Parede interior; Revestimento de tetos
Info
PROBEX AQUOSO (cor CAMBALA TD 290) - Verniz para madeira em exterior
N/A
Ano: 2021
Autor(es): entidade LNEC
Keywords: Documento de aplicação; Verniz; Revestimento por pintura; Proteção de madeiras; Madeira
Info
TINTA ACRÍLICA PURA 9G (cor branca) + PRIMÁRIO PLIOMIL AQUOSO - Revestimentos por pintura para paredes exteriores
N/A
Ano: 2021
Autor(es): entidade LNEC
Keywords: Documento de aplicação; Revestimento de paredes; Revestimento por pintura; Parede exterior
Info
Tinta SUPERLAVÁVEL MATE + Primário ISOSELANTE - Revestimento por pintura para paredes e tetos interiores de edifícios
N/A
Ano: 2021
Autor(es): entidade LNEC
Keywords: Documento de aplicação; Revestimento de paredes; Revestimento por pintura; Parede interior; Revestimento de tetos
Info
TINTA NOVÁQUA HD + PRIMÁRIO CINOLITE - Revestimentos por pintura para paredes exteriores
N/A
Ano: 2020
Autor(es): entidade LNEC
Keywords: Documento de aplicação; Revestimento por pintura; Parede exterior; Revestimento de parede
Info
Tinta DYRUSTAR (cor branca) + Primário Aquoso Branco - Revestimento por pintura de base aquosa para paredes e tetos interiores de edifícios
N/A
Ano: 2019
Autor(es): entidade LNEC
Keywords: Documento de aplicação; Revestimento de parede; Revestimento por pintura; Parede interior; Revestimento de teto
Info
Luso Spray Branco - Produto para marcação rodoviária
N/A
Ano: 2018
Autor(es): entidade LNEC
Keywords: Europa; Termoplástico; Pavimento betuminoso; Marca rodoviária
Info
MILACRIL BRILHANTE (cor branca) e PRIMÁRIO TT - Revestimento por pintura para superfícies cerâmicas no interior de habitações
N/A
Ano: 2018
Autor(es): entidade LNEC
Keywords: Documento de aplicação; Revestimento de paredes; Revestimento por pintura; Parede interior; Revestimento de tetos
Info
TINTA AQUAREPEL (cor branca) - Revestimentos por pintura para paredes exteriores
N/A
Ano: 2018
Autor(es): entidade LNEC
Keywords: Documento de aplicação; Revestimento por pintura; Parede exterior; Revestimento de paredes
Info
TINTA DYRUSTAR (cor branca) + PRIMÁRIO AQUOSO BRANCO - Revestimento por pintura de base aquosa para paredes e tetos interiores de edifícios
N/A
Ano: 2018
Autor(es): entidade LNEC
Keywords: Documento de aplicação; Revestimento de paredes; Revestimento por pintura; Parede interior; Revestimento de tetos
|